Add Item to Cart:
APPLICATION GUIDELINES
Application temperature: Above 55°F
Open assembly time: 5 minutes (70°F/50% RH)(
Total assembly time: 10-15 minutes (70°F/50% RH)
Minimum required spread: Approximately 6 mils or 250 square feet per gallon.
Required clamping pressure: Enough to bring joints tightly together (generally, 100-150 psi for softwoods, 125-175 psi for medium woods and 175-250 psi for hardwoods)
Methods of application: Easily spread with a roller spreader or brush, or may be transferred to plastic bottles for finer gluing applications.
Cleanup: Damp cloth while glue is wet. Scrape off and sand dried excess.
Temperature | Strength psi | % wood failure |
---|---|---|
Room Temperature | 3,750 | 72 |
150°F Overnight | 1,750 | 6 |
LIMITATIONS
Not for continuous submersion or for use below the waterline. Not for structural or load bearing applications. Use when temperature, glue and materials are above 50°F. Freezing may not affect the function of the product but may cause it to thicken. Agitation should restore product to original form. Because of variances in the surfaces of treated lumber, it is a good idea to test for adhesion. Read MSDS before use.
NOTE: KEEP FROM FREEZING.
KEEP OUT OF THE REACH OF CHILDREN
Corporate Office: Häfele America Co., 3901 Cheyenne Drive, Archdale, N.C. 27263 Phone: 800.423.3531, Fax: 800.325.6197, Local Phone: 336.434.2322, Email: info@haefeleamericas.com |