APPLICATION GUIDELINES
Application temperature: Above 47°F
Open assembly time: 8-10 minutes (70°F/50% RH)(
Total assembly time: 20-25 minutes (70°F/50% RH)
Minimum required spread: Approximately 6 mils or 250 square feet per gallon.
Required clamping pressure: Enough to bring joints tightly together (generally, 100-150 psi for softwoods, 125-175 psi for medium woods and 175-250 psi for hardwoods)
Methods of application: Plastic bottles for fine applications; glue may also spread with a roller spreader or brush.
Cleanup: Damp cloth while glue is wet. Scrape off and sand dried excess.
BOND STRENGTH ASTM D-905 (On Hard Maple)
Temperature | Strength psi | % wood failure |
---|
Room Temperature | 4,000 | 57 |
150°F Overnight | 800 | 0 |
LIMITATIONS
Not for continuous submersion or for use below the waterline. Not for structural or load bearing applications. Use when temperature, glue and materials are above 45°F. Store product below 75°. Storage above this temperature may cause product to thicken and reduce the usable shelf life. If thickened, shake vigorously by firmly tapping the bottle on a hard a surface until the product is restored to original form. Because of variances in the surfaces of treated lumber, it is a good idea to test for adhesion. For best results gluing exterior doors or exotic and oily woods, please contanct our Technical Support Team at 1-800-347-4583. Read MSDS before use.
NOTE: KEEP FROM FREEZING.
KEEP OUT OF THE REACH OF CHILDREN