APPLICATION GUIDELINES
Application temperature: Above 50°F
Assembly time after glue application: 5 minutes (70°F/50% RH)
Minimum required spread: 7 mils (typical)
Required clamping pressure: Enough to bring joints tightly together (generally, 30-80 psi for HPL, 100-150 psi for softwoods, 125-175 psi for medium woods and 175-250 psi for hardwoods).
Methods of application: Easily spread with a roller spreader or brush, or may be transferred to plastic bottles for finer gluing application.
Cleanup: Damp cloth while glue is wet. Scrape off dried excess.
BOND STRENGTH ASTM D-905 (On Hard Maple)
Temperature | Strength psi | % wood failure |
---|
Room Temperature | 3,600 | 77 |
150° Overnight | 1,600 | 10 |
LIMITATIONS
Not intended for exterior use or where moisture is likely. For exterior applications use Titebond II Premium Wood Glue. Freezing may not affect the function of the product, but may cause it to thicken. Agitation should restore product to original form.
KEEP FROM FREEZING
Note
Chalk temperature indicates the lowest approximate temperature at which the glue, air or materials to be bonded may be to assure a good bond.