APPLICATION GUIDELINES
Application temperature: Above 50°F
Assembly time after glue application: 5 minutes (70°F/50% RH)
Total assembly time: 10-15 minutes (70°F/50% RH)
Minimum required spread: 7 mils (typical)
Required clamping pressure: Enough to bring joints tightly together (generally, 30-80 psi for HPL, 100-150 psi for softwoods, 125-175 psi for medium woods and 175-250 psi for hardwoods)
Methods of application: Easily spread with a roller spreader or brush, or may be transferred to plastic bottles for finer gluing applications.
Cleanup: Damp cloth while glue is wet. Scrape off and sand dried excess.
BOND STRENGTH ASTM D-905 (On Hard Maple)
Temperature | Strength psi | % wood failure |
---|
Room Temperature | 3,550 | 50 |
150°F Overnight | 1,600 | 15 |
Titebond White Glue is not intended for exterior use or where moisture is likely. For exterior applications Titebond III Ultimate Wood Glue or Titebond II Premium Wood Glue. Not for structural or load beaing applications. Do not use when temperature, glue or materials are below 50°. Freezing may not affect the function of the product but may cause it to thicken. Agitation should restore product to original form. Read MSDS before use. KEEP FROM FREEZING.